Superalloys have become an increasingly important part of the cobalt supply chain. Superalloys are the largest source of cobalt demand behind battery applications. They are used in both commercial and defence aerospace applications. In 2025, cobalt demand from superalloys reached 20kt, up 7.5%, supported by increased defence spending, as assessed by Benchmark’s Cobalt Service. While cobalt-containing superalloys service a wide range of end markets, aerospace is the largest, accounting for 58% of cobalt demand from superalloys, approximately 11.5kt in 2025.